#33
|
||||
|
||||
|
Nice work.
Going to tackle my transom now that the snow is melting. Questions; How much arjay did you use? What are those metal standoff things that appear to be spacing the skins? You used poly resin. Is it OK to use epoxy with arjay? I plan to cut the inside skin 3" from the corners, dig out wood, glass the old skin back in using epoxy resin. All of my fiberglassing experience is with epoxy. I read that it is best for "repairs" of old glass and has better adhesive qualities. Did you pour it solid and re-drill holes for drains? Any problems/suggestions? Thanks for any suggestions you can make.
__________________
1984 V20 "Express" & 2003 Suzuki DF140 (SOLD!) 2000 GradyWhite 265 Express YouTube/SkunkBoat https://www.youtube.com/channel/UC4F...znGospVOD6EJuw Transom Rebuild https://www.youtube.com/watch?v=EEz94NbKCh0 https://www.youtube.com/watch?v=Oe_ZmPOUCNc |
|
|