#1
|
|||
|
|||
|
Take a drill bit and ream them out just a little to clean out any caulk or other stuff. I then would get that stuff made by West System which is a white powder which thickens up resin and will add strength. Tape over one side of hole and fill. May take a couple of times to get it nice and smooth.
|
![]() |