For the crazy best shine......just 2 steps

1. 3M # 05996 Machine Polish............damp ( not wet ) wool applicator, slow speed buffer approx. 4' sections at a time. Take your time, pattern the buffer across, then up down re covering the same areas. Wipe off excess, and move to next section.
When entire hull is done, just wash the hull off with hose and car soap. Don't waste time and energy buffing.

THEN apply.................

2. Un Finish Car Polish ( orange container )
Hand apply with clean, damp rag, liberally - meaning don't be cheap with it...
Do a section, then hand buff off with clean T shirt or such cotton ....
If you want, then do a light wipe of entire hull with a separate slightly damp rag to remove any excess etc.

WOW - your boat will shine like crazy!!
People will say, holly SH, that shine is SICK !!!

And, best of all the Nu Finish lasts longer than ANYTHING I've tried, and I've tried all kinds of products from pure Carnuba to other crap available.

3-6 months later, just another light application of the Nu Finish to keep it going.
Reply With Quote
  #2  
Unread 08-24-2016, 09:56 AM
Cruiser35 Cruiser35 is offline
Junior Member
 
Join Date: Jul 2016
Posts: 1
Default

I used the same compound with very good results then applied 3M Scotch guard by hand- super easy and looks great
Reply With Quote
  #3  
Unread 09-15-2016, 08:57 PM
steplift20 steplift20 is offline
God
 
Join Date: Nov 2004
Location: Beautiful New Jersey the high taxes state
Posts: 3,042
Default

Ok guys and fellow wellcraft owners, I own my baby for over 20 years and I think I finally found out how to use color restorer, you know the stuff the brings back some of ghetto shine lost to the sun and everything else out there, ok this is what I found out, I used to put it on and wait for it to haze then rub rub rub it off and you can see marks on the gellcoat so what I find was I put it on and wiped it off, worked out great Try it and let me know if I'm right or as usual wrong again but it worked for me
__________________
love to fish
Reply With Quote
  #4  
Unread 10-07-2016, 04:27 PM
000's's Avatar
000's 000's is offline
Member
 
Join Date: Aug 2010
Location: Tappahannock,Va
Posts: 64
Default

Wax is the worst thing to use . Look at a surf board the wax builds up turns yellow - same thing happens to a boat ! Clean the pain buff the hell out of it - 3m over rated - McGuires does just as good job and costs a lot less - finish with ultimate paint guard plus - 2 coats 12 hrs apart - then see what u think of wax - oh yeah use it on aluminum and glass -
__________________
Capt. Fred Hill
www.PirateRepublic.net
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 07:42 PM.


Powered by vBulletin® Version 3.8.2
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.