The stuff is amazing!!!! And super strong especially with multiple layup and you change the fiber direction. I built my entire boat with it it wrapped every curve on my boat.
|
|
#2
|
||||
|
||||
|
do you use fairing compound over it before paint?
__________________
1984 V20 "Express" & 2003 Suzuki DF140 (SOLD!) 2000 GradyWhite 265 Express YouTube/SkunkBoat https://www.youtube.com/channel/UC4F...znGospVOD6EJuw Transom Rebuild https://www.youtube.com/watch?v=EEz94NbKCh0 https://www.youtube.com/watch?v=Oe_ZmPOUCNc |
|
#3
|
||||
|
||||
|
Yes it will need to be faired before primer and paint. I just barely bump grind the cloth then apply fairing compound as needed. Dont grind out to much you will lose strength. On this repair i had some thickened resin left so i slicked the repair with what i had left just to use it up.
|
|
#4
|
|||
|
|||
|
Quote:
|
|
#5
|
||||
|
||||
|
Looking good and good advice all. You'll be happier with the transom at 25 inches.
__________________
1985 Wellcraft V-20, Evinrude ETEC 150: SOLD 1979 Marine Trader 44, twin Ford Lehman 120s 2006 Panga 14, Tohatsu 20 |
|
#6
|
||||
|
||||
|
How many layers of glass did you lay on the outside of the repair to bring it even? I'm going to be raising the transom on my Grady to 25" as well.
__________________
1999 Wellcraft 22WA-200 Ocean Runner 1982 Grady White Tarpon 190-110 Evinrude-Sold 1996 Striper 2100WA-RIP Sandy 1989 Wellcraft 18-Sport-125 Force-sold |
|
#7
|
||||
|
||||
|
The last layer of 1708 is the only layer thats meets the edge were i stopped grinding. Every other layer is progressive. Meaning i have 4 layers that build up the ply veneer then 2 final layers......the first of the final outside layer falls short from the grinding by like 4 inches....the last and final layer is the only one that meets the grind edge. It lets you progressively build up your thickness with out having all the thickness at the imediate edge. Hopefully that makes sense.
|
|
#8
|
||||
|
||||
|
The trick to the clear bubble free 90 degree curves is to build up some thickened (fumed silica,cabosil) resin on the outside corners then lay your cloth down and wet it out like usual when you hit the corners with the bubble popper (roller) its like magic when spread the thickened resin under the cloth.
|
|