Cleaned out the holes (where 5200 was) filled with formula 27 let dry and sanded.

Peeled the 2 top pin stripes off, now I just have to get the water line decal off and install new water line tape.

Then I'll be ready for installation of the Poli-glo.

Heading to Lowes to pick up some new numbers and letters for boat ID (I want as much as possible to look new) and find some stuff to help peel the waterline tape off. Heat gun didn't do a great job on the part I tried but did ok on the small pin stripes. I think 3m makes something if I remember.

Then heading to Wallyworld to get a new battery and bilge pmp for the Jon boat. Never a dull moment or moment a boat doesn't cost u something. BOAT = break out another thousand.

battery $30.00, motor 1,600, bilge pmp 30.00 nailing the main muff in the boat PRICELESS!!!
__________________
Tis better to be quiet and thought a fool than open your mouth and prove it!!

1991 V-20 cuddy I/O 350 volvo duo prop, 1998 15ft Grumman 9.9 Johnson
Reply With Quote
 

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 05:29 AM.


Powered by vBulletin® Version 3.8.2
Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.