Today's post is light on pics as my hands were gloved and mixing/spreading thickened epoxy today. But I finished up all the grinding yesterday and today set to placing the first layer of the transom:
I think I'll grab some larger mixing tubs from Home Depot on the way home from work tomorrow. Mixing up the thickened epoxy in quart size tubs is a chore. It takes a lot more material than I anticipated to thicken up a batch. Time to do some math and see if I have enough Cabosil and milled fiber to do all the peanut buttering I have left to do.
Also need to order another 20 grinding discs to cover the grinding I'll have to do on the sole as well. For anyone embarking on a similar project a word of advice - don't think that 24 grit is too aggressive like I did before starting. After grinding out the hull, if there was a lower grit I'd jump on it. I went through 20 discs and I was pushing thru with discs that should have been swapped out much sooner. If I had 40 to do the hull grinding I would have used them all and had no regrets. This isn't a cheap endeavour and just like FG and resin, grinding discs are not a place to skimp if you enjoy your sanity.