Found local 4x8 i/2 kiln dried treated ply from local boat builder. $80. He'll sell me what i need , 30"x43". But its still $80. Probably gonna go with that.
Was thinking cabosil to bond wood to hatch, then seal all with couple of layers of 6 oz.

Any thoughts

I thought it was a little overkill, greyduk, but it sure saved a lot of itching.

Thanks for the tip,step. Was wondering how to avoid drips. Luckily i have a large piece of starboard to us as a work table and i have to repaint deck afterwards anyway.