Ok. I see. Make a template out of PVC board. "Laminate" that. Seperate those 2 and tab the inner skin in then fill. Seems like a good plan. I guess I can make some sort of jig to curve the template as I glass it then use it again to reinforce the inner skin while I pour.
Unfortunately I haven't gotten to touch the boat this weekend. Trying to shorten the infinite honey-do list as much as I can so when I order $1000 work of fiberglass and core material maybe it will ease the burn. Probably not though.