Quote:
Originally Posted by carboncow
Laim,
more questions...
1. What did you use to cut your deck? We used a circular saw that cut like butter but can only get an inch or so to the wall...the zip saw is not as fun.
I used a circular saw where i could and then a sawzall in the corners
2. Could you expend on the "more weight" and "trap moisture" comment, I guess I'm not seeing/understand that (but I am listening!).
One deck on top of another is 2 times the weight( a considerable amount) and if one is sandwiched on top of the other you will likely get voids and use a ton of resin to bond them together(more weight/cost).The underside of the deck should be allowed air to reach it,allow it to breathe and extend its life,you want to put a layer of glass on the underside of the new deck core also
3. How do you suggest the foam comes out? I think I read a guys post on using a chain saw and my buddy is a chain saw master. So do we think the foam adds to the shortness of life of stringers due holding the moisture in the area?
I used a shovel,flat bar and then a scraper and finally grinding disc,most of it comes out easily,chainsaw is gonna make a lot of mess and may damge the hull if not careful
yes i believe the foam decreases the life of a wood cored stringer
4. Do you suggest trying to salvage the fiberglass from the stringers as much as posible and just insert more wood?
Cut the fibreglass about 1 inch up from where it meets the hull all the way along the stringer and then remove all the old stringer,cut new stringers to size and use the cleaned out channel you left as a guide to insert the new stringer on thickened resin,then glass the whole thing in with 1708.
A new layer of 1708 will seal you new stringers better than the fibreglass job they did at thew factory
5. What kind of wood are using for the stringers? Based on their height we are expecting to find plywood in there too!
|
I used 3/4 exterior grade fir doubled up,marine ply is better but cost is way higher,IMO properly sealed fir will last nearly as long. I am not sure what the original stringer material is on your year,mine was spruce but it is a 1973,others may chime in here