Quote:
Originally Posted by Destroyer View Post
Proper primer for aluminum is zinc chromate. Two coats, first coat up and down, second coat side to side..that way there are no highlights. There are several other types also, including epoxies, but the US Navy uses zinc chromate ... and most of their equipment seems to get a lot of salt usage for some reason.
Good info. Thanks Destroyer.