Material was 1/2 inch marine grade ply and resin. The wet look is the resin pre putting the cap back on. A little wet to help the cap adhear.
Once the cap went on I put a bunch of sand bags and 5 gallon pails on it to keep it from having bubbles.
Sorry, meant Durabak and my process was. Layed some of the textured durabak that I had left over from the floor. Then sanded it down a little to take the rough peaks out. Finally painted with the smooth version of Durabak.
|
Thanks..actually sounds lie you made The whole thing easier (not easy)
Genius move on sanding the Durabak some and repainting...