View Full Version : 5200
charlie_the_tuna
05-25-2008, 12:32 PM
how long does this crap take to set?
 
shot it last night about 7:30pm and its still wet as hell.
tsubaki
05-25-2008, 01:05 PM
Your time, about 2 weeks, our time about 2 days.
Humidity and temp. (all day & overnight) plays more into the cureing than getting some from a prom date.
Try to find the fast cure, it might be more suited to the upper latitudes.
http://i175.photobucket.com/albums/w159/tsubaki3/Picture087.jpg
THEFERMANATOR
05-25-2008, 01:39 PM
Should set within 24-48 hours, but takes 7-10 days to cure. Moisture doesn't hurt the cure time, but cold does.
macojoe
05-25-2008, 09:46 PM
Next time get the fast cure!!
randlemanboater
05-26-2008, 07:33 AM
I hate 5200.
cterrebonne
05-26-2008, 06:23 PM
3m  could make alot of money if they sold a 5200 kit. it would include a box of disposable shop towels and a can of acetone. haha
phatdaddy
05-26-2008, 07:16 PM
i can order that stuff on the phone and get it on my fingers..............
lumberslinger178
05-26-2008, 07:37 PM
i can order that stuff on the phone and get it on my fingers..............
I could be walking down the street , look across the street , see it in the front window of the hardware store , and still get it all over me.:you:
garagenc
05-28-2008, 03:08 PM
hit it with water
Stinky_Hooker
05-29-2008, 11:51 AM
FYI dont you fastcure for LARGE areas, like tank hatches and such if the gap is big. It will blister badly...I ony like fastcure for small jobs like sealing screws, hindged and deck hatches and such.
 
 
Its drying slowly because its supposed to...in the world of glue the longer it takes the tougher it is....
phester
05-29-2008, 07:36 PM
what would be the preferred material for the gas tank cover? The gap all around is about a light 1/8" and it was smutched neatly in there 3/4" deep. It was still white and soft and came out pretty easy.[I thought it was going to be a horror.] How about the 4200 uv?, or anything uv?
spareparts
05-30-2008, 06:45 AM
I use the 4000 everywhere topside with good luck
Stinky_Hooker
05-30-2008, 08:16 AM
Id use 5200 on it...Ive never used the 4000 as spare says, but Im sure its good stuff if he is using it.
 
 
Also on the 5200 (or any caulk for hatches) run you a piece of heavy mono like 100-130# all the way around under the caulk and in one corner out of the way leave a small tag sticking out. This way you can pull it and cut the caulk if you have to.
THEFERMANATOR
05-30-2008, 10:01 AM
The 4000 would be better for a hatch cover for the fact it will seal it, but not permanently. 5200 can be some tough stuff to get off later. 4000 is meant to seal, whereas 5200 is meant to seal and be an adhesive.
randlemanboater
05-30-2008, 10:20 AM
I used the clear 3m marine silicon sealer on my gas hatch when I knew I was going to have to go back in fairly soon.  It was much more secure than I thought it was going to be, I had to work pretty hard to open the hatch again.
fishingwithblue
05-30-2008, 12:19 PM
i can order that stuff on the phone and get it on my fingers..............
:you:I just thought about re-sealing some inspection plates and got it on my hands.
macojoe
05-30-2008, 01:32 PM
I used 4200 on mine I hope I don't ever have o take i up!
phester
05-30-2008, 06:59 PM
yeah, I don't think there is a need for the 5200, my concern is uv tolerant.....would hate to see a few weeks down the road all that chaulk getting yellow/brown discolor from the sun. My floor looks factory new now. Now that I think about it, doesn't the 4000 say UV right on the label?? BTW, thanks for the input fellas.
THEFERMANATOR
05-30-2008, 08:34 PM
4000 is more UV resistant than 5200 the last I checked. 5200 is really meant for bonding and sealing below the waterline, 4000 is meant for hatches and portholes.
Airslot
05-30-2008, 09:49 PM
Yes, there is 4200, 5200, and 4000UV
phester
05-31-2008, 05:34 AM
4000UV it is . Hopefully it come in tube for the chaulking gun, rather than s hand squeeze tube.
vBulletin® v3.8.2, Copyright ©2000-2025, Jelsoft Enterprises Ltd.