tsubaki
09-09-2007, 03:00 PM
Felt I needed to replace the thru hull fittings in the bow.
http://i175.photobucket.com/albums/w159/tsubaki3/P3160382.jpg
http://i175.photobucket.com/albums/w159/tsubaki3/P3160381.jpg
Noticed a small crack beginning in one of the fittings.
http://i175.photobucket.com/albums/w159/tsubaki3/thurhullfitting.jpg
But got to thinking the best coarse would be to just fill the holes.
http://i175.photobucket.com/albums/w159/tsubaki3/Picture003-1.jpg
http://i175.photobucket.com/albums/w159/tsubaki3/Picture002-2.jpg
Cut a couple pieces of ½ “ thick glass and bolted with 10/24 flat heads, countersunk, * *locknutted, and 5200ed.
http://i175.photobucket.com/albums/w159/tsubaki3/Picture004-2.jpg
Then filled the holes with Evercoat and finished off with Marine Tex.
http://i175.photobucket.com/albums/w159/tsubaki3/Picture006-1.jpg
Think I’ll walk down to the dock while the Marine Tex cures out to see what I can aggravate. ;D ;D
http://i175.photobucket.com/albums/w159/tsubaki3/Picture005-1.jpg
http://i175.photobucket.com/albums/w159/tsubaki3/P3160382.jpg
http://i175.photobucket.com/albums/w159/tsubaki3/P3160381.jpg
Noticed a small crack beginning in one of the fittings.
http://i175.photobucket.com/albums/w159/tsubaki3/thurhullfitting.jpg
But got to thinking the best coarse would be to just fill the holes.
http://i175.photobucket.com/albums/w159/tsubaki3/Picture003-1.jpg
http://i175.photobucket.com/albums/w159/tsubaki3/Picture002-2.jpg
Cut a couple pieces of ½ “ thick glass and bolted with 10/24 flat heads, countersunk, * *locknutted, and 5200ed.
http://i175.photobucket.com/albums/w159/tsubaki3/Picture004-2.jpg
Then filled the holes with Evercoat and finished off with Marine Tex.
http://i175.photobucket.com/albums/w159/tsubaki3/Picture006-1.jpg
Think I’ll walk down to the dock while the Marine Tex cures out to see what I can aggravate. ;D ;D